Carbonaceous materials for the production of aluminium - Anodes, cathodes blocks, sidewall blocks and baked ramming pastes - Determination of the thermal conductivity using a comparative method


ISO 12987:2004 specifies a method for the determination of thermal conductivity of carbonaceous material in the temperature range of 20 °C to 60 °C. The typical range of thermal conductivity for these materials is 2 W/(K·m) to 100 W/(K·m).

This method can be used for other carbon materials, such as graphitized electrodes for other applications.


CONTENT PROVIDER
International Organization for Standardization [iso]

Others Also Bought
Carbonaceous materials used in the production of aluminium -- Baked anodes and sidewall blocks -- Determination ...
Carbonaceous materials used in the production of aluminium -- Baked anodes -- Determination of the reactivity to ...
Carbonaceous materials for the production of aluminium - Baked anodes - Determination of the air permeability
Document History
We have no document history for this standard.
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.