TAPPI/ANSI T 826 om-21

Short span compressive strength of containerboard

This method describes a procedure for determining the compressive resistance of containerboard.

This method is intended for containerboard having a span-to-thickness ratio of 5 or less. This is equivalent to a grammage of between approximately 100 g/m² (20 lb/1000 ft²) (1) and 440 g/m² (90 lb/1000 ft²).