ASTM B601-12

Standard Classification for Temper Designations for Copper and Copper Alloys—Wrought and Cast


1.1 This classification establishes temper designations for copper and copper alloys???wrought and cast. The temper designations are classified by the process or processes used in manufacturing the product involved and its resulting properties. It is not a specification of copper and copper alloys.

1.2 The property requirements for the tempers are given in the applicable product specification.


CONTENT PROVIDER
ASTM International [astm]

Others Also Bought
Standard Specification for Cartridge Brass Sheet, Strip, Plate, Bar, and Disks
Standard Specification for General Requirements for Wrought Copper and Copper-Alloy Rod, Bar, Shapes and Forg ...
Standard Specification for General Requirements for Wrought Copper Alloy Wire
Document History
Revises:
Revised By:
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.