SAE AMS 2759/7E-2021

Carburizing and Heat Treatment of Carburizing Grade Steel Parts

This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements and procedures for three classes of gas, vacuum, liquid, and low pressure (LPC) carburizing and related heat treatment of parts fabricated from carburizing grade steels. Parts made from steels other than those specified in the detail specifications may be heat treated in accordance with the applicable requirements using processing temperatures, times, and other parameters recommended by the material producer unless otherwise specified by the purchaser. This specification does not cover pack carburizing.


Content Provider
Society of Automotive Engineers [sae]


Others Also Bought

Gas Nitriding of Low-Alloy Steel Parts
Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)
Steel, Corrosion Resistant, Bars, Wire, Forgings, Rings, and Extrusions 15Cr - 4.5Ni - 0.30Cb (Nb) - 3.5Cu Consumable ...
Document History
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.
ANSI Logo

As the voice of the U.S. standards and conformity assessment system, the American National Standards Institute (ANSI) empowers its members and constituents to strengthen the U.S. marketplace position in the global economy while helping to assure the safety and health of consumers and the protection of the environment.

CUSTOMER SERVICE
NEW YORK OFFICE
ANSI HEADQUARTERS