Historical

T 826

Short span compressive strength of containerboard

This method is intended for containerboard having a span-to-thickness ratio of 5 or less. This is equivalent to a grammage of between approximately 100 g/m2 (20 lb/1000 ft2) (1) and 440 g/m2 (90 lb/1000 ft2).