Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies


1.1 Steel assemblies and subassemblies fabricated by welding, such as composite structural members, sash, weldments, etc., that are to be hot-dip galvanized after fabrication, are subject to warpage and distortion of the material due to the heating and cooling integral to the galvanizing operation, particularly when it is necessary for the assembly to be dipped more than once to coat the entire surface.

1.2 This specification is applicable in either inch pounds or SI units. Inch pounds and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in parentheses.

1.3 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


CONTENT PROVIDER
ASTM International [astm]

Others Also Bought
Standard Practice for Providing High-Quality Zinc Coatings (Hot-Dip)
Standard Specification for Zinc (Hot-Dip Galvanized) Coatings on Iron and Steel Products
Standard Practice for Safeguarding Against Embrittlement of Hot-Dip Galvanized Structural Steel Products and ...
Included in Packages
This standard is not included in any packages.
Document History
Amendments & Corrections
We have no amendments or corrections for this standard.