SAE AMS 5344F-2007 (SAE AMS5344F-2007)

Steel, Corrosion Resistant, Investment Castings 16Cr 4.1Ni 0.28Cb 3.2Cu Homogenization, Solution and Precipitation Heat Treated (H900) 180 ksi (1241 MPa) Tensile Strength (17-4)


This specification covers a corrosion-resistant steel in the form of investment castings. These castings have been used typically for parts requiring good corrosion resistance and strength up to 600 \mDF (316 \mDC), but usage is not limited to such applications. Certain processing procedures and service conditions may cause these castings to become subject to stress-corrosion cracking; APR1110 recommends practices to minimize such conditions.


CONTENT PROVIDER
Society of Automotive Engineers [sae]

Others Also Bought
Steel, Corrosion Resistant, Investment Castings 16Cr 4.1Ni 0.28Cb 3.2Cu Homogenization and Solution Heat Treated ...
Steel, Corrosion Resistant, Investment Castings 16Cr 4.1Ni O.28Cb 3.2Cu, Homogenization, Solution, and Precipitation ...
Steel, Corrosion Resistant, Investment Castings 16Cr 4.0Ni 0.28Cb 3.2Cu, Homogenization, Solution, and Precipitation ...
Document History
Revised By:
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.