SAE AMS 5355J-2009 (SAE AMS5355J-2009)

Steel, Corrosion Resistant, Investment Castings 16Cr 4.1Ni 0.28Cb 3.2Cu Homogenization and Solution Heat Treated or Homogenization, Solution, and Precipitation Heat Treated


This specification covers a corrosion-resistant steel in the form of investment castings. These castings have been used typically for parts requiring good corrosion resistance and strength up to 600 \mDF (316 \mDC), but usage is not limited to such applications. Certain processing procedures and service conditions may cause these castings to become subject to stress-corrosion cracking; ARP1110 recommends practices to minimize such conditions. Where stress-corrosion is considered to be a factor, precipitation heat treatment should be performed at a temperature not lower than 1000 \mDF (538 \mDC).


CONTENT PROVIDER
Society of Automotive Engineers [sae]

Others Also Bought
Liquid Salt Bath Ferritic Nitrocarburizing Non-Cyanide Bath
Steel, Corrosion Resistant, Investment Castings 16Cr 4.1Ni 0.28Cb 3.2Cu Homogenization, Solution and Precipitation ...
Steel, Corrosion-Resistant, Investment Castings, 16Cr - 4.1Ni - 0.28Cb (Nb) - 3.2Cu, Homogenization, Solution, ...
Document History
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.