SAE AMS 5709H-2008 (SAE AMS5709H-2008)

Nickel Alloy, Corrosion and Heat Resistant, Bars and Forgings 58Ni 19.5Cr 13.5Co 4.3Mo 3.0Ti 1.4Al 0.05Zr 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975\mDF (1079\mDC) Solution, Stabilization, and Precipitation Heat Treated


This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, and forging stock. These products have been used typically for parts, such as pins, nuts, and turbine blades, requiring high strength up to 1500 \mDF (816 \mDC) and oxidation resistance up to 1750 \mDF (954 \mDC), but usage is not limited to such applications.