Most recent

SAE AMS 5709J-2019

Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated


This specification covers a corrosion and heat-resistant nickel alloy in the form of bars, forgings, and forging stock.


CONTENT PROVIDER
Society of Automotive Engineers [sae]

Document History
Included in Packages
This standard is not included in any packages.
Amendments & Corrections
We have no amendments or corrections for this standard.